Matches in DBpedia 2016-04 for { ?s ?p "Slow strain rate testing (SSRT), also called constant extension rate tensile testing (CERT), is a standard method of testing of materials, often metals, in which the specimen is subjected to elongation at a constant rate. The load is varied to maintain the constant extension rate. While extended, the material is exposed to an environment (temperature, specific fluid, etc.). The method evaluates the corrosion behaviour of the material in the given environment, often the environmental effects on the material fracture or stress-corrosion cracking susceptibility."@en }
Showing triples 1 to 2 of
2
with 100 triples per page.
- Slow_strain_rate_testing abstract "Slow strain rate testing (SSRT), also called constant extension rate tensile testing (CERT), is a standard method of testing of materials, often metals, in which the specimen is subjected to elongation at a constant rate. The load is varied to maintain the constant extension rate. While extended, the material is exposed to an environment (temperature, specific fluid, etc.). The method evaluates the corrosion behaviour of the material in the given environment, often the environmental effects on the material fracture or stress-corrosion cracking susceptibility.".
- Q17105850 abstract "Slow strain rate testing (SSRT), also called constant extension rate tensile testing (CERT), is a standard method of testing of materials, often metals, in which the specimen is subjected to elongation at a constant rate. The load is varied to maintain the constant extension rate. While extended, the material is exposed to an environment (temperature, specific fluid, etc.). The method evaluates the corrosion behaviour of the material in the given environment, often the environmental effects on the material fracture or stress-corrosion cracking susceptibility.".